Репозиторий Евразийского национального университета имени Л.Н. Гумилева
Репозиторий Евразийского национального университета имени Л.Н. Гумилева
Репозиторий Евразийского национального университета имени Л.Н. Гумилева
Просмотр элемента 
  •   Главная
  • Научные статьи
  • 01. Публикации в изданиях зарубежных стран
  • Environmental Science
  • Просмотр элемента
  •   Главная
  • Научные статьи
  • 01. Публикации в изданиях зарубежных стран
  • Environmental Science
  • Просмотр элемента
JavaScript is disabled for your browser. Some features of this site may not work without it.

Production of Soft Magnetic Materials Fe-Si and Fe-Si-Al from Blends of Red Muds and Several Additives: Resources for Advanced Electrical Devices

Thumbnail
Автор
Khanna, Rita
Konyukhov, Yuri
Zinoveev, Dmitri
Li, Kejiang
Maslennikov, Nikita
Burmistrov, Igor
Kargin, Jumat
Kravchenko, Maksim
Mukherjee, Partha Sarathy
Дата
2025
Редактор
Sustainability
ISSN
2071-1050
xmlui.dri2xhtml.METS-1.0.item-identifier-citation
Khanna, R.; Konyukhov, Y.; Zinoveev, D.; Li, K.; Maslennikov, N.; Burmistrov, I.; Kargin, J.; Kravchenko, M.; Mukherjee, P.S. Production of Soft Magnetic Materials Fe-Si and Fe-Si-Al from Blends of Red Muds and Several Additives: Resources for Advanced Electrical Devices. Sustainability 2025, 17, 1795. https://doi.org/10.3390/ su17051795
Аннотации
The present study developed a novel approach for transforming red mud (RM) into soft magnetic materials (SMMs) for applications in advanced electrical devices in the form of Fe-Si and Fe-Si-Al alloys. A total of ten blends were prepared based on two RMs, three iron oxide additives (Fe2O3, black and red mill scales), alumina and carbonaceous reductants in a range of proportions. Carbothermic reduction of the blends was carried out in a vertical Tamman resistance furnace at 1600–1650 ◦C for 30 min in an argon atmosphere; synthetic graphite was used as a reductant. Reaction products were characterized using scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), X-ray fluorescence (XRF) and X-ray diffraction (XRD). Significant amounts of Fe-rich metallic droplets/regions of different grain sizes (0.5 to 500 µm) were produced in these studies. The formation of Fe-Si alloys with Si contents from 3.9 to 6.7 wt.% was achieved in 8 out of 10 blends; the optimal levels of Si for SMMs ranged from 3.2 to 6.5 wt.%. There was clear evidence for the formation of Fe-Si-Al (up to 1.8 wt.% Al) alloys in 4 out of 10 blends. In addition to lowering operating challenges associated with RM processing, blending of RMs with iron oxide additives and alumina presents a novel recycling approach for converting RMs into valuable SMMs for possible emerging applications in renewable energy, storage, electrical vehicles and other fields. Along with reducing RM stockpiles across the globe, this approach is expected to improve resource efficiency, mitigating environmental impacts while generating economic benefits.
URI
http://repository.enu.kz/handle/enu/29945
Открыть
Production of Soft Magnetic Materials Fe-Si and Fe-Si-Al from.pdf (7.533Mb)
Collections
  • Environmental Science[350]
Показать полную информацию
CORE Recommender

Евразийский национальный университет имени Л.Н. Гумилева | Научная библиотека | Контакты
YM
Научная библиотека | Контакты
 

Просмотр

Весь DSpaceСообщества и коллекцииДата публикацииАвторыНазванияТематикаЭта коллекцияДата публикацииАвторыНазванияТематика

Моя учетная запись

ВойтиРегистрация

Евразийский национальный университет имени Л.Н. Гумилева | Научная библиотека | Контакты
YM
Научная библиотека | Контакты