Concentration polarization and ionic conductivity of nanocomposite thermoelectric materials K0.01Cu1.94S, K0.02Cu1.94S, K0.03Cu1.94S

Показать сокращенную информацию

dc.contributor.author Kubenova, M. M.
dc.contributor.author Balapanov, M. Kh.
dc.contributor.author Kuterbekov, K. A.
dc.contributor.author Akhmetgaliev, B.
dc.contributor.author Ishembetov, R. Kh.
dc.date.accessioned 2024-12-26T07:40:10Z
dc.date.available 2024-12-26T07:40:10Z
dc.date.issued 2024
dc.identifier.issn 2522-9869
dc.identifier.other doi.org/10.32523/ejpfm.2024080105
dc.identifier.uri http://rep.enu.kz/handle/enu/20444
dc.description.abstract The paper presents experimental results of concentration polarization and ionic conductivity of nanocomposite thermoelectric materials K0.01Cu1.94S , K0.02Cu1.94S , K0.03Cu1.94S . According to X-ray phase analysis, the synthesized samples are monoclinic jarleite Cu1.93÷1.97S with an admixture of oxygen oxide Cu2S and monoclinic chalcocyte. High values of total ionic conductivity are observed, ranging from 0.86 to 1.5 Cm/cm. The lowest ionic conductivity (0.86 Cm/cm at 355 ◦ C) is observed for alloy K0.02Cu1.94S . In addition, it was found that with an increase in the concentration of potassium in the studied materials, ionic conductivity tends to decrease, activation energy increases, but the characteristics of ion transport remain high, corresponding to superionic materials. ru
dc.language.iso en ru
dc.publisher Eurasian Journal of Physics and Functional Materials ru
dc.relation.ispartofseries Volume 8 Number 1;
dc.subject ionic conductivity ru
dc.subject nanocomposite ru
dc.subject superionic semiconductors ru
dc.subject activation energy ru
dc.title Concentration polarization and ionic conductivity of nanocomposite thermoelectric materials K0.01Cu1.94S, K0.02Cu1.94S, K0.03Cu1.94S ru
dc.type Article ru